Close up image of patterned cracking in the surface of the paint film resembling the scales of an alligator.

Causes

  • Painting a warm surface in direct sunlight.
  • Application of oil-based or alkyd paint over a damp or wet surface.
  • Moisture escaping through the exterior walls (less likely with latex paint than with oil-based or alkyd paint).
  • Exposure of latex paint film to dew, high humidity or rain shortly after paint has dried, especially if there was inadequate surface preparation.

Solutions

  • Determine if blisters are attributed to heat or moisture by opening the blisters and examining the backside of blistered paint.
  • If only the most recent paint applied has blistered, the blister was probably caused by heat. Remove blisters by scraping, then sanding; prime any bare wood and repaint with a high-quality exterior paint in the desired sheen.
  • If blisters go down to the substrate, the blister was probably caused by moisture. In this case, remove blisters and more importantly remove the source of moisture. Prime all bare areas with a high-quality primer. Repaint the surface with a high-quality paint in the desired finish.

READY TO GET STARTED?

Contact a Behr Pro Rep Icon

CONTACT A BEHR PRO® REP

Your reputation depends on your ability to do the job right. BEHR can help.

Find a rep
Technical Services Icon

TECHNICAL SERVICES

1-800-661-1591
Mon - Fri, 6am-3pm PST
Sat. & Sun., Closed

PRO XTRA logo

JOIN THE HOME DEPOT® PRO XTRA LOYALTY PROGRAM

Get 10% - 20% Back in Quarterly Rewards
BEHR® Paints, Stains & Primers.

sign up on homedepot.ca