Causes

  • Application of too heavy a coat of paint.
  • Application in excessively humid and/or cool conditions.
  • Application of over thinned paint
  • Airless spraying with the gun too close to the substrate being painted, or moving the gun too slowly.
  • Application over a glossy, slick surface that does not provide sufficient “tooth” for the new paint to stick.

Solutions

  • If the paint is still wet, immediately brush out or re-roll to redistribute the excess evenly.
  • If the paint has dried, sand and reapply a new coat of top quality paint.
  • Correct any unfavorable conditions: do not thin the paint; avoid cool or humid conditions; sand glossy surfaces.
  • Two coats of paint at the recommended spread rate are better than one heavy coat, which can also lead to sagging. Consider removing doors to paint them supported horizontally.

READY TO GET STARTED?

Contact a Behr Pro Rep Icon

CONTACT A BEHR PRO® REP

Your reputation depends on your ability to do the job right. BEHR can help.

Find a rep
Technical Services Icon

TECHNICAL SERVICES

1-800-661-1591
Mon - Fri, 6am-3pm PST
Sat. & Sun., Closed

PRO XTRA logo

JOIN THE HOME DEPOT® PRO XTRA LOYALTY PROGRAM

Get 10% - 20% Back in Quarterly Rewards
BEHR® Paints, Stains & Primers.

sign up on homedepot.ca